From: Dr. Guillermo A. Morales (morales$##$combichemlab.com)
Date: Tue Jul 04 2000 - 10:28:57 EDT


Hi bin,

Well, I'm sure you already tried this, but one way to increase the loading
is trying double coupling.

If you tried the coupling using N-protected (Fmoc or tBoc) amino acid and
DCI in DCM and that didn't work well, another way to try is converting the
hydroxyl unit of the polymer support into a bromide using PPh3 and CBr4 in
DMF for 2-3 hours, then treat the brominated resin with N-protected amino
acid adding CsI or NaI in DMF or DMA.

I hope this helps.

Guillermo.
-----
Guillermo A. Morales
Morales Consulting
E-mail: morales$##$combichemlab.com
Website: http://www.combichemlab.com
Member of the Combi-Web Consortium: http://www.combi-web.com

-----Original Message-----
From: owner-orglist$##$dq.fct.unl.pt [mailto:owner-orglist$##$dq.fct.unl.pt]On
Behalf Of bin hu
Sent: Tuesday, July 04, 2000 7:13 AM
To: Multiple recipients of list orglist
Subject: None

hi!all you orglist members
      Who is working in solid phase synthesis of peptide?Would you please
give me some advice in this field?
I am using Benzylamine Resin as solid support,HMBA(hydroxymethylated
benzoic acid) as Linker.I have met an problem in improving loading of the
first amino acid.
     Thanking and waiting for your reply!

________________________________________________________________________
Get Your Private, Free E-mail from MSN Hotmail at http://www.hotmail.com

__________________

ORGLIST - Organic Chemistry Mailing List
Website / Archive / FAQ: http://www.orglist.net/
List coordinator: Joao Aires de Sousa (jas$##$mail.fct.unl.pt)

__________________

ORGLIST - Organic Chemistry Mailing List
Website / Archive / FAQ: http://www.orglist.net/
List coordinator: Joao Aires de Sousa (jas$##$mail.fct.unl.pt)


Date view Thread view Subject view Author view Attachment view

This archive was generated by hypermail 2.1.4 : Fri Sep 19 2003 - 12:15:35 EDT